Non-amagqabi Ukucoleka kunye mhlophe Aluminiyam Paste |I-Aluminiyam Pigment

Non-amagqabi Ukucoleka kunye mhlophe Aluminiyam Paste |I-Aluminiyam Pigment


  • Igama Eliqhelekileyo:I-Aluminiyam yokuCola
  • Elinye Igama:Ncamathelisa i-Aluminiyam Pigment
  • Udidi:Umbala-Ibala-Pigment yeAluminiyam
  • Imbonakalo:Ulwelo lwesilivere
  • Inombolo yeCAS: /
  • Inombolo ye-EINECS: /
  • Ifomula yemolekyuli: /
  • Igama lebrand:Colorcom
  • Indawo yemvelaphi:eTshayina
  • Beka ubomi kwishelufa:Iminyaka eyi-1
  • Iinkcukacha zeMveliso

    Iithegi zeMveliso

    Inkcazo:

    I-Aluminiyam yePaste, yintsimbi yebala eyimfuneko.Amacandelo ayo aphambili yi-snowflake aluminium particles kunye ne-petroleum solvents ngendlela yokunamathisela.Kungemva kwetekhnoloji yokulungiswa okukhethekileyo kunye nonyango lomphezulu, ukwenza umphezulu we-aluminium flake ugudileyo kunye nomphetho osicaba ucocekile, ukumila okuqhelekileyo, ukugxininiswa kobungakanani bamasuntswana, kunye nokuhambelana okugqwesileyo kunye nenkqubo yokwambathisa.I-Aluminiyam Paste inokohlulwa ibe ngamacandelo amabini: uhlobo lwamagqabi kunye nohlobo olungamagqabi.Ngexesha lokugaya, enye i-asidi enamafutha ithathelwa indawo yenye, eyenza i-Aluminiyam Paste ibe neempawu ezihluke ngokupheleleyo kunye nembonakalo, kwaye iimilo ze-aluminium flakes ziyi-snowflake, isikali seentlanzi kunye nedola yesilivere.Ikakhulu isetyenziswa kwiinqwelo zeemoto, iiplastiki ezibuthathaka, iingubo zentsimbi zemizi-mveliso, iingubo zaselwandle, iingubo ezichasene nobushushu, iingubo zokuphahla njalo njalo.Ikwasetyenziswa kwipeyinti yeplastiki, ihardware kunye nepeyinti yesixhobo sasekhaya, ipeyinti yesithuthuthu, ipeyinti yebhayisekile njalo njalo.

    Iimpawu:

    Ngobukhulu besuntswana elicolekileyo kakhulu, ukusabalalisa okumxinwa, ukuguda, kunye nomgubo ofihlakeleyo omangalisayo, uthotho alufaki nje ukuqaqamba okuhle, kodwa kunye nesiphumo esigqibeleleyo somgangatho omhlophe kunye nomhlophe.

    Isicelo:

    Isetyenziswa kakhulu ekucokiseni iimoto, isithuthuthu, ithoyizi, iingubo zamashishini ngokubanzi, iingubo zaselwandle, ii-inki zokuprinta, njl.

    Inkcazo:

    IBanga

    Isiqulatho esingaguquguqukiyo (±2%)

    Ixabiso le-D50 (±2μm)

    Uhlalutyo lweSkrini <45μm min.(%)

    Specific Gravity malunga.(g/cm3)

    Isinyibilikisi

    LS502

    65

    2

    99.9

    1.5

    MS/SN

    LS505

    65

    5

    99.9

    1.5

    MS/SN

    LS507

    65

    7

    99.9

    1.5

    MS/SN

    LS509

    65

    9

    99.9

    1.5

    MS/SN

    LG430

    65

    30

    99.9

    1.5

    MS/SN

    I-LG419

    65

    19

    99.9

    1.5

    MS/SN

    I-LG418

    65

    18

    99.9

    1.5

    MS/SN

    I-LG417

    65

    17

    99.9

    1.5

    MS/SN

    I-LG415

    65

    15

    99.9

    1.5

    MS/SN

    I-LG414

    65

    14

    99.9

    1.5

    MS/SN

    I-LG413

    65

    13

    99.9

    1.5

    MS/SN

    I-LG412

    65

    12

    99.9

    1.5

    MS/SN

    NS509

    65

    9

    99.9

    1.5

    MS/SN

    NS415

    65

    15

    99.9

    1.5

    MS/SN

    Amanqaku:

    1. Nceda uqinisekise ukuba uqinisekise isampuli phambi kokusetyenziswa ngakunye kwe-aluminium yesilivere yokunamathisela.
    2. Xa usasaza intlama ye-aluminium-silver, sebenzisa indlela yokusasaza kwangaphambili: khetha isinyibilikisi esifanelekileyo kuqala, yongeza isinyibilikisi kwintlama ye-aluminium-silver kunye nomlinganiselo we-aluminium-silver intlama kwi-solvent njenge-1: 1-2, yixube. kancinci kwaye ngokulinganayo, kwaye emva koko ugalele kwizinto ezisisiseko ezilungiselelwe.
    3. Gwema ukusebenzisa izixhobo zokusasaza ngesantya esiphezulu ixesha elide ngexesha lokuxuba.

    Imiyalelo yokugcina:

    1. Intlama ye-aluminiyam yesilivere kufuneka igcine isikhongozeli sivaliwe kwaye ubushushu bokugcina kufuneka bugcinwe ku-15℃-35℃.
    2. Kuphephe ukuchanabeka ngokuthe ngqo kwilanga elithe ngqo, imvula kunye nobushushu obugqithisileyo.
    3. Emva kokungatywinwa, ukuba kukho nayiphi na intlama ye-aluminium yesilivere eseleyo kufuneka itywinwe ngokukhawuleza ukuphepha ukuqhuma kwe-solvent kunye nokusilela kwe-oxidation.
    4. Ukugcinwa kwexesha elide le-aluminium yesilivere ye-paste ingaba yi-solvent volatility okanye enye ungcoliseko, nceda uphinde uvavanye ngaphambi kokusetyenziswa ukuze ugweme ilahleko.

    Amanyathelo kaxakeka:

    1. Kwimeko yomlilo, nceda usebenzise umgubo wekhemikhali okanye isanti ekhethekileyo eyomileyo ukucima umlilo, ungasebenzisi amanzi ukucima umlilo.
    2. Ukuba intlama yesilivere ye-aluminium ingena ngengozi emehlweni, nceda uhlambe ngamanzi ubuncinane imizuzu eyi-15 kwaye ufune iingcebiso zonyango.