Cobalt Sulfate |10124-43-3
Inkcazo yeMveliso:
Into | IBanga leCatalyst | Electroplating Grade | IBanga loShishino |
Co | ≥21.0% | ≥20.5% | ≥20.5% |
Nickel(Ni) | ≤0.001% | ≤0.002% | ≤0.002% |
Intsimbi (Fe) | ≤0.001% | ≤0.002% | ≤0.002% |
Magnesium (Mg) | ≤0.001% | ≤0.002% | ≤0.002% |
Icalcium (Ca) | ≤0.001% | ≤0.002% | ≤0.002% |
IManganese(Mn) | ≤0.001% | ≤0.002% | ≤0.002% |
IZinc (Zn) | ≤0.001% | ≤0.002% | ≤0.002% |
Isodium (Na) | ≤0.001% | ≤0.002% | ≤0.002% |
Ubhedu (Cu) | ≤0.001% | ≤0.002% | ≤0.002% |
I-Cadmium (Cd) | ≤0.001% | ≤0.001% | ≤0.001% |
Izinto ezinganyibilikiyo zamanzi | ≤0.01% | ≤0.01% | ≤0.01% |
Ingcaciso yeMveliso:
Cobalt Sulfate, rose-red crystal.Umgubo obomvu emva kokuphelelwa ngamanzi emzimbeni, unyibilika emanzini kunye ne-methanol, unyibilika kancinci kwi-ethanol.Indawo yokunyibilika (°C): 96 ~ 98 Ubuninzi obunxulumeneyo (amanzi = 1): 1.948 (25 °C) Indawo yokubila (°C): 420 (-7H2O) Ukufudumala ukuya kuma-420 °C ukuphulukana namanzi asixhenxe ekristale.Imozulu ilula emoyeni.
Isicelo:
Isetyenziswa njenge arhente yokomisa ipeyinti kushishino lwepeyinti.Isetyenziswa njengombala we-porcelain glaze kushishino lweceramic.Umzi mveliso wemichiza wokwenza i-cobalt-containing pigments kwaye njengento ekrwada yokuveliswa kweetyuwa ezahlukeneyo ze-cobalt.Ishishini lebhetri njengeebhetri zealkaline kunye nezongezo zeLide powder.Ukongeza, ikwasetyenziswa njenge-catalyst kunye ne-reagent yokuhlalutya.Isetyenziswe kwi-cobalt ye-electroplating, ukwenza ibhetri yokugcina, i-cobalt pigment, i-ceramics, i-enamel, i-glaze, kwaye isetyenziswe njenge-catalyst, i-foam stabiliser, i-ejenti yokomisa.
Iphakheji: 25 kgs / ibhegi okanye njengoko ucela.
Ugcino: Gcina kwindawo engenamoya, eyomileyo.
Umgangatho wesiGqeba: uMgangatho waMazwe ngaMazwe.